In 1995 251 x 10 9 lb cl2 lb 261 x 10 9 lb naoh 261

Info iconThis preview shows page 1. Sign up to view the full content.

View Full Document Right Arrow Icon
This is the end of the preview. Sign up to access the rest of the document.

Unformatted text preview: the source of NaOH and Cl2. In 1995 25.1 x 10 9 lb Cl2 lb 26.1 x 10 9 lb NaOH 26.1 lb 5 Electrolysis of Aqueous CuCl2 Electrolysis of Aqueous CuCl2 Anode (+) Eo = -1.36 V -1.36 2 Cl- ---> Cl 2(g) + 2e---> Cathode (-) Eo = +0.34 V +0.34 Cu2+ + 2e- ---> Cu 2eEo for cell = -1.02 V for Note that Cu is more + easily reduced than either H 2O or Na +. Anode 6 electrons BATTERY electrons BATTERY Cathode Cl- Na+ H2O Also the source of NaOCl for use in bleach. Cathode Cl- Cu2+ H2O Page 1 Producing Aluminum Producing Aluminum 2 Al2O3 + 3 C ---> 4 Al + 3 CO 2 ---> 7 Charles Hall (1863-1914) developed electrolysis process. Founded Alcoa. Page 2...