NINGBO STAR C2S - g/m 2 55 PLY Bonding J/m 2 150 Test...

Info iconThis preview shows page 1. Sign up to view the full content.

View Full Document Right Arrow Icon
NINGBO STAR C2S Art Board Basis Weigh t Thickness Stiffness (Taber 15 o ) g/m 2 24"x36 " mN · m ( ± 10%) ± 3 % 500 (lb) μ m ( ± 4% ) pt ( ± 4% ) C D MD 18 0 11 1 185 7. 3 1. 4 2.5 20 0 12 3 210 8. 3 1. 6 3.0 21 0 12 9 220 8. 7 2. 1 3.5 23 0 14 1 250 9. 8 2. 8 4.6 25 0 15 4 275 10. 8 3. 6 6.2 27 0 16 6 305 12. 0 5. 0 7.8 30 0 18 4 355 14. 0 7. 0 12.0 35 0 21 5 410 16. 1 10. 0 18.0 40 0 24 6 470 18. 5 16. 0 26.0 Propert y Uni t Value PPS (Top/Back) μ m 1.4 Moistur e % 6 ± 1.5 Brightness (Top/Back ) % 93.0 ± 2 75 ° Gloss(Top/Back) % 66
Background image of page 1
This is the end of the preview. Sign up to access the rest of the document.

Unformatted text preview: g/m 2 55 PLY Bonding J/m 2 150 Test condition (ISO): temp 23 1 o C, relative humidity 50 2% Note: Shaded substances are non-regular substances which are not produced regularly. Date: 15 July 2008 PDF "pdfFactory Pro" www.fineprint.com.cn...
View Full Document

This note was uploaded on 11/03/2011 for the course REAL ESTAT 83676 taught by Professor Unknown during the Spring '97 term at Golden Gate.

Ask a homework question - tutors are online